Join 60,000+ competitive exam aspirants
Name the welding defect in which we observe a long and continuous visual separation line between the base metal and the heat affected zone.
Incomplete fusion
Lamellar tearing
Undercut
Hot cracking
Lamellar tearing
Lamellar tearing is a welding defect characterized by a terraced fracture occurring beneath the weld, primarily in the base metal. It appears as a long, continuous separation line that runs parallel to the rolling plane of the plate, specifically separating the base metal from the heat-affected zone (HAZ) due to high through-thickness strains.
ISO 5817:2014; AWS D1.1
Lamellar tearing is a welding defect characterized by a terraced fracture occurring beneath the weld, primarily in the base metal. It appears as a long, continuous separation line that runs parallel to the rolling plane of the plate, specifically separating the base metal from the heat-affected zone (HAZ) due to high through-thickness strains.
╧ГzтАЛ=AFтАЛ тАФ Where ╧ГzтАЛ is the through-thickness stress and A is the cross-sectional area of the base metal.
╧╡zтАЛ=L0тАЛ╬ФLтАЛ тАФ Where ╧╡zтАЛ represents the through-thickness strain exceeding the material's ductility limit.
This defect occurs in materials with poor through-thickness ductility, typically due to the presence of non-metallic inclusions like elongated manganese sulfides (MnS). When the weld metal cools and contracts, it exerts high tensile stress in the through-thickness direction (Z-direction) of the plate. If the plate cannot deform plastically to accommodate this shrinkage, the inclusions crack, leading to a stepwise or continuous separation of the metal layers.
Primarily occurs in thick plates where high weld shrinkage stresses are restrained.
Associated with high concentrations of sulfur and elongated silicate inclusions.
Common in T-joints and corner joints under heavy restraint.
Can be mitigated by using cleaner steels with low sulfur content (S<0.005%) and calcium treatment to modify inclusion shape.
Incomplete fusion (Option A) occurs when the weld metal fails to bond with the base metal or preceding bead surface, usually at the root or side wall.
Undercut (Option C) is a surface groove melted into the base metal at the toe of the weld, usually due to excessive current or travel speed.
Hot cracking (Option D) is a solidification crack occurring during the cooling stage at temperatures near the solidus point, often due to high residual stresses and composition impurities.
B is correct тАФ Lamellar tearing is a classic through-thickness fracture defect resulting from high localized shrinkage stresses in materials with low Z-direction ductility.
Always remember that Lamellar tearing is unique because it happens in the base metal, not the weld metal itself, often identifiable by its step-like or 'terraced' appearance.