Join 60,000+ competitive exam aspirants
Which aggregate type has been reported to achieve strength up to 125 MPa with a water-cement ratio of 0.32?
Natural gravel
Crushed stone aggregate
ALAG (Cementitious aggregate)
Recycled aggregate
ALAG (Cementitious aggregate)
ALAG is a synthetic, cementitious aggregate manufactured to be physically and chemically compatible with the cement paste. By improving the interfacial transition zone (ITZ) and minimizing strength-limiting micro-cracks, it allows for high-strength concrete performance that conventional natural aggregates struggle to achieve.
IS 383:2016 (General Guidelines for Aggregates)
ALAG is a synthetic, cementitious aggregate manufactured to be physically and chemically compatible with the cement paste. By improving the interfacial transition zone (ITZ) and minimizing strength-limiting micro-cracks, it allows for high-strength concrete performance that conventional natural aggregates struggle to achieve.
fckтАЛ=APтАЛ тАФ Compressive strength calculation representing load P over cross-sectional area A
w/c=Mass┬аof┬аCementMass┬аof┬аWaterтАЛ тАФ Water-cement ratio governing hydration and density
The strength of high-strength concrete is limited by the bond between the aggregate and the cement paste. ALAG aggregates possess a textured, porous surface that promotes a stronger mechanical interlock and potential chemical bonding with the mortar, reducing the stress concentrations typically found at the ITZ of natural rounded gravels.
ALAG is specifically designed for high-strength and wear-resistant applications.
A w/c ratio of 0.32 is considered very low, necessitating the use of high-performance aggregates to reach 125 MPa.
Natural aggregates often suffer from poor adhesion, limiting concrete strength in the ultra-high performance range.
Superior bond strength at the aggregate-paste interface
High abrasion resistance and durability
Significant reduction in permeability
Higher unit cost compared to natural crushed stone
Availability is limited to specialized industrial suppliers
Industrial flooring
High-strength structural columns
Heavy-duty pavements
Natural gravel (Option A) is often unsuitable for >100 MPa concrete due to its smooth surface texture limiting bond.
Recycled aggregates (Option D) typically result in lower strength than virgin aggregates due to the porous adhered mortar.
Standard normal-strength concrete typically uses a w/c ratio between 0.40 and 0.55.
C is correct тАФ ALAG (Cementitious aggregate) is engineered to enhance the interfacial transition zone, enabling compressive strengths up to 125 MPa at a low water-cement ratio of 0.32.
In competitive exams, remember that as the target compressive strength increases (>80 MPa), the quality and physical properties of the aggregate become as critical as the cementitious material properties.